Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 45.8 kN/m | 261 pli | Die B, post cured- 4 hours at 177°C; ASTM D624 |
Multibase C6-150 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 45.8 kN/m | 261 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-540 Dow-Corning Class VI Elastomer Information provided by Multibase |