Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | >= 45.0 kN/m | >= 257 pli | Method B; ISO 34 |
S&E Specialty Polymers XP23-566-1 PVC Description: PVC weatherable, integral colored, filledApplication: Low gloss lift gate molding compound which meets Chrysler MSDC 543.Information provided by S&E Specialty Polymers |
|||
Tear Strength | 45.0 kN/m | 257 pli | D624 |
Polykemi AB POLYelast TPE Z900 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tear Strength | 45.0 kN/m | 257 pli | |
Huntsman IROGRAN® A 78 P 4766 NM Ether-Based TPU-For Cable Industry TransparentInformation provided by Huntsman |
|||
Tear Strength | >= 45.0 kN/m | >= 257 pli | DIN 53507 |
Karina 802-06/77-Y-BZ Blue PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 45.0 kN/m | 257 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 4640 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tear Strength | 45.0 kN/m | 257 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 4660 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tear Strength | 45.0 kN/m | 257 pli | Die B |
Momentive Performance Materials Silplusâ„¢ 70 HS High Strength Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | Die C; ISO 34-1B |
Lubrizol Advanced Materials PEARLCOAT® Activa D118K Thermoplastic Polyurethane Elastomer PEARLCOAT® Activa D118K is a polycaprolactone copolyester based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss asp.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | ASTM D2240 |
UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tear Strength | 45.0 kN/m | 257 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | DIN 53515 |
Lubrizol ESTANE® 5702F3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 45.0 kN/m | 257 pli | with incision; ISO 34B |
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | ISO 34/1 |
A. Schulman INVISION™ VX-5085UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5085UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 85 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-990 (MT) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | DIN 53515 |
Lubrizol ESTANE® 5702F2 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 45.0 kN/m | 257 pli | DIN 53515 |
Lubrizol ESTANE® 58201 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 45.0 kN/m | 257 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 5049-110 TPE, Modified Injection Molding Grade for Auto Mud Flaps The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 5049-110 is specifically designe.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | ASTM D624 |
ELASTO UK Dryflex® 650900 TPE, Improved Compression Set and High Temperature Resistance, 90A Hardness The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | notched; ASTM D624 (C) |
Arkema Group Pebax® 3533 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Tear Strength | 45.0 kN/m | 257 pli | DIN ISO 34-1/Bb |
BASF Elastollan C 75 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tear Strength | >= 45.0 kN/m | >= 257 pli | ISO 34 |
Austin Novel Materials Texalan® 265A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tear Strength | >= 45.0 kN/m | >= 257 pli | ISO 34 |
Austin Novel Materials Texalan® 470A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tear Strength | 45.0 kN/m | 257 pli | |
Trelleborg R721 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 45.0 kN/m | 257 pli | ISO 34-B |
AlphaGary Evoprene™ G 975 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Tear Strength | 45.0 kN/m | 257 pli | DIN 53515 |
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 45.0 kN/m | 257 pli | DIN 53515 |
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 45.0 kN/m | 257 pli | DIN 53515 |
Lubrizol ESTANE® T5083 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | >= 45.0 kN/m | >= 257 pli | DIN 53507 |
Karina 70/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |