Mechanical Properties | Metric | English | Comments | |
---|---|---|---|---|
Tear Strength | 29.8 kN/m | 170 pli | ASTM D624 | |
Multibase Multi-Flex® TPE A 6900 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
||||
Tear Strength | 29.8 kN/m | 170 pli | ASTM D624 | |
Multibase Multi-Flex® TPE A 7321 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
||||
Tear Strength | 29.8 kN/m | 170 pli | ASTM D412 | |
Multibase TPSiV™ 3010-60A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
||||
Tear Strength | 29.8 kN/m | 170 pli | ASTM D412 | |
Multibase TPSiV™ 3040-60A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
||||
Tear Strength | 29.8 kN/m | 170 pli | ASTM D624 | |
PolyOne Dynaflex™ G7670-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7670-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
||||
Tear Strength | 29.8 kN/m | 170 pli | Die C, 510 mm/min; ASTM D624 | |
PolyOne Geon™ Vinyl Flexible A6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
||||
Tear Strength | 29.8 kN/m | 170 pli | Die C, 510 mm/min; ASTM D624 | |
PolyOne Geon™ Vinyl Flexible B65T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
||||
Tear Strength | 29.8 - 114 kN/m | 170 - 650 pli | Average value: 67.6 kN/m Grade Count:16 | |
Overview of materials for PVC, Transparent This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M.. |
||||
Tear Strength | 29.8 kN/m | 170 pli | Die C, 510 mm/min; ASTM D624 | |
PolyOne Elastamax™ HTE 1104 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
||||
Tear Strength | 29.8 kN/m | 170 pli | ASTM D624 | |
Multibase Multi-Flex® G 7150 TPE Styrene Ethylene Butylene Styrene Block Copolymer Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInforma.. |
||||
Tear Strength | 29.8 kN/m | 170 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 | |
Multibase C6-235 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
||||
Tear Strength | 29.8 kN/m | 170 pli | Die B,post cured- 2 hours at 177°C; ASTM D624 | |
Multibase C6-250 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
||||
Tear Strength | 29.8 kN/m | 170 pli | ASTM D624 | |
Multibase Multi-Flex® A 7101 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
||||
Tear Strength | 29.8 kN/m | 170 pli | ASTM D624 | |
Multibase Multi-Flex® A 7206 E TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
||||
Tear Strength | 29.8 kN/m | 170 pli | ASTM D624 | |
STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1060 TPE Product Description: StarCLEAR CLR-1060 is an easy processing TPE designed for injection molding. Soft and ultra clear TPEs specifically targeted to medical, consumer and sporting goods market. Feat.. |
||||
Tear Strength | 29.8 kN/m | 170 pli | ASTM D624 | |
Teknor Apex Telcar® TL-6800-73 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
||||
Tear Strength | 29.8 kN/m | 170 pli | ASTM D624 | |
Teknor Apex UNIPRENE® 7100-73 Thermoplastic Elastomer Information provided by Teknor Apex Company |
||||
Tear Strength | 29.8 kN/m | 170 pli16 % | 16 % | 200% elongation; ASTM D412 |
Lubrizol ESTANE® 58219 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance, low temperature performance and clarity. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection .. |
||||
Tear Strength | 29.8 kN/m | 170 pli | Trouser; ASTM D470 | |
Lubrizol ESTANE® 54600 Ester Based Thermoplastic Polyurethane Features: Very good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion Available in Americas, Europe,.. |
||||
Tear Strength | 29.8 kN/m | 170 pli | ||
Dow Corning HV 1520/40 40 Shore Hardness Conductive liquid silicone rubber with high tear strength, high electrical conductivity and fast cure speedInformation provided by Dow Corning |
||||
Tear Strength | 29.8 kN/m | 170 pli | ASTM D624 | |
Diamond Polymers Softflex® 2701-1502R Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
||||
Tear Strength | 29.8 kN/m | 170 pli | ASTM D624 | |
Diamond Polymers Softflex® SF 5060 Overmold for Nylon Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
||||
Tear Strength | 29.8 kN/m | 170 pli | ISO 34-1 | |
Alliance Polymers Viprene™ G44A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G44A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
||||
Tear Strength | 29.8 kN/m | 170 pli | ISO 34-1 | |
Alliance Polymers Viprene™ G44A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G44A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
||||
Tear Strength | 29.8 kN/m | 170 pli | ASTM D470 | |
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b.. |
||||
Tear Strength | 29.8 kN/m | 170 pli | Die C (graves), 20 in/min; ASTM D624 | |
PolyOne Synprene® ST-6240 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Over-Molding GradeUV StabilizedApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |