Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 18.0 kN/m | 103 pli | ISO 34-1 |
PolyOne OnFlex™ S FR 40A-3S1841 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2610 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | Die B |
Momentive Performance Materials TSE 221-6U Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/70 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | |
Trelleborg B573 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | |
Trelleborg E566 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tear Strength | 18.0 kN/m | 103 pli | |
Trelleborg E569 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ASTM D624 |
ELASTO UK Dryflex® 500450S SEBS Based Material, Unfilled Qualities, 45A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ASTM D624 |
ELASTO UK Dryflex® 502400S SEBS Based Material, Unfilled Qualities, 40A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ASTM D624 |
ELASTO UK Dryflex® 502450S SEBS Based Material, Unfilled Qualities, 45A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ASTM D624 |
ELASTO UK Dryflex® 602400S SEBS Based Material, Filled Qualities, 40A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ASTM D624 |
ELASTO UK Dryflex® 602450S SEBS Based Material, Filled Qualities, 45A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ASTM D624 |
ELASTO UK Dryflex® 600450S SEBS Based Material, Filled Qualities, 45A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ASTM D 624 |
API Megol AM DP2392/40 SEBS Adhesion Modified Overmolding for Polar Polymers Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tear Strength | 18.0 - 35.0 kN/m | 103 - 200 pli | ASTM D 624 |
API Megol AM SV/PS SEBS Adhesion Modified Overmolding for PS Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tear Strength | 18.0 kN/m | 103 pli | Die B |
Momentive Performance Materials TUFEL™ III 92506 Biocompatible Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | Die B |
Momentive Performance Materials FSE7560 Heat Cured Fluorosilicone Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ISO 34-B |
AlphaGary Evoprene™ GC 5697 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ISO 34-B |
AlphaGary Evoprene™ Super G 947 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |