Mechanical Properties Metric English Comments
Modulus of Rupture 0.0004905 - 0.000981 GPa

@Temperature 500 °C,
Time 10800 sec
0.07114 - 0.142 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories INCT-50S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0004905 - 0.000981 GPa

@Temperature 500 °C,
Time 10800 sec
0.07114 - 0.142 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories INCT-80N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.0004905 - 0.000981 GPa

@Temperature 1000 °C,
Time 10800 sec
0.07114 - 0.142 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories MIX-2 Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.85e-7 - 0.000981 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000558 - 0.142 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PT-165 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.85e-7 - 0.000981 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000558 - 0.142 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PT-170 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.85e-7 - 0.000981 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000558 - 0.142 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PTA-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.85e-7 - 0.000981 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000558 - 0.142 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PTA-180 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.85e-7 - 0.000981 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000558 - 0.142 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PTF-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 3.85e-7 - 0.000981 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000558 - 0.142 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories PTC-130S Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved