Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.012753 GPa @Temperature 1350 °C, Time 10800 sec |
1.8497 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories A40 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.012753 GPa @Temperature 1000 °C, Time 10800 sec |
1.8497 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HSC-16SF-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.012753 GPa @Temperature 1500 °C, Time 10800 sec |
1.8497 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories HSC-17 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.012753 - 0.015696 GPa @Temperature 1500 °C, Time 10800 sec |
1.8497 - 2.2765 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories PTF-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.012753 GPa @Temperature 1350 °C, Time 10800 sec |
1.8497 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories SFC-165 High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |