Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00883 GPa @Temperature 1500 °C |
1.28 ksi @Temperature 2730 °F |
|
Sharadaa Ceramics REFCAST K High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Modulus of Rupture | 0.00883 GPa @Temperature 1500 °C |
1.28 ksi @Temperature 2730 °F |
|
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Modulus of Rupture | 0.00883 GPa @Temperature 1500 °C |
1.28 ksi @Temperature 2730 °F |
|
Sharadaa Ceramics REFINSUL 15 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Modulus of Rupture | 0.00883 GPa @Temperature 1500 °C |
1.28 ksi @Temperature 2730 °F |
|
Sharadaa Ceramics REFINSUL 15LI Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Modulus of Rupture | 0.00883 GPa @Temperature 1500 °C |
1.28 ksi @Temperature 2730 °F |
|
Sharadaa Ceramics REFINSUL 9 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Modulus of Rupture | 0.00883 GPa @Temperature 1500 °C |
1.28 ksi @Temperature 2730 °F |
|
Sharadaa Ceramics REFCAST HA PLUS High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |