Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.006867 GPa @Temperature 110 °C, Time 86400 sec |
0.9960 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories A64 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 GPa @Temperature 110 °C, Time 86400 sec |
0.9960 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories APC-100G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 GPa @Temperature 500 °C, Time 10800 sec |
0.9960 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories APC-120G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 GPa @Temperature 110 °C, Time 86400 sec |
0.9960 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories APC-50G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 GPa @Temperature 1400 °C |
0.9960 ksi @Temperature 2550 °F |
|
Chosun Refractories CRAG-S27 Long Stopper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 GPa @Temperature 1400 °C |
0.9960 ksi @Temperature 2550 °F |
|
Chosun Refractories CRAG-S50 Long Stopper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 GPa @Temperature 1400 °C |
0.9960 ksi @Temperature 2550 °F |
|
Chosun Refractories CRAG-S50 Long Stopper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 - 0.010791 GPa @Temperature 110 °C, Time 86400 sec |
0.9960 - 1.5651 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HACT-180G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 - 0.010791 GPa @Temperature 1000 °C, Time 10800 sec |
0.9960 - 1.5651 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HACT-180G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 GPa @Temperature 1350 °C, Time 10800 sec |
0.9960 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories LPCT-16DS Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 GPa @Temperature 110 °C, Time 86400 sec |
0.9960 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories LPCT-18PI Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 GPa @Temperature 110 °C, Time 86400 sec |
0.9960 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories MMCT-75 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 GPa @Temperature 1000 °C, Time 10800 sec |
0.9960 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories SFC-70R High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 GPa @Temperature 1000 °C, Time 10800 sec |
0.9960 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories SW87 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 GPa @Temperature 1500 °C, Time 10800 sec |
0.9960 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories SW88 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.006867 GPa @Temperature 110 °C, Time 86400 sec |
0.9960 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories TCH-165Y Torpedo Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |