Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0004905 - 0.000981 GPa @Temperature 500 °C, Time 10800 sec |
0.07114 - 0.142 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories INCT-50S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0004905 - 0.000981 GPa @Temperature 500 °C, Time 10800 sec |
0.07114 - 0.142 ksi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories INCT-80N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.0004905 - 0.000981 GPa @Temperature 1000 °C, Time 10800 sec |
0.07114 - 0.142 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories MIX-2 Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.85e-7 - 0.000981 GPa @Temperature 110 °C, Time 86400 sec |
0.0000558 - 0.142 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.85e-7 - 0.000981 GPa @Temperature 110 °C, Time 86400 sec |
0.0000558 - 0.142 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PT-170 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.85e-7 - 0.000981 GPa @Temperature 110 °C, Time 86400 sec |
0.0000558 - 0.142 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PTA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.85e-7 - 0.000981 GPa @Temperature 110 °C, Time 86400 sec |
0.0000558 - 0.142 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PTA-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.85e-7 - 0.000981 GPa @Temperature 110 °C, Time 86400 sec |
0.0000558 - 0.142 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PTF-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 3.85e-7 - 0.000981 GPa @Temperature 110 °C, Time 86400 sec |
0.0000558 - 0.142 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories PTC-130S Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |