Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00735 GPa @Temperature 110 °C |
1.07 ksi @Temperature 230 °F |
|
Sharadaa Ceramics REFINSUL 15LI Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Modulus of Rupture | 0.00735 GPa @Temperature 1100 °C |
1.07 ksi @Temperature 2010 °F |
|
Sharadaa Ceramics REFINSUL 8S Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Modulus of Rupture | 0.00735 GPa @Temperature 1100 °C |
1.07 ksi @Temperature 2010 °F |
|
Sharadaa Ceramics THERMO PATCH EXCEL High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Modulus of Rupture | 0.00735 GPa @Temperature 110 °C |
1.07 ksi @Temperature 230 °F |
|
Sharadaa Ceramics REFCAST HA PLUS High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |