Mechanical Properties Metric English Comments
Modulus of Rupture 0.000981 - 0.001962 GPa

@Temperature 1000 °C,
Time 10800 sec
0.142 - 0.2846 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories GUN-140L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.000981 - 0.001962 GPa

@Temperature 500 °C,
Time 10800 sec
0.142 - 0.2846 ksi

@Temperature 932 °F,
Time 3.00 hour
Chosun Refractories INCT-100N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.000981 GPa

@Temperature 1500 °C,
Time 10800 sec
0.142 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories M55 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.000981 - 0.0024525 GPa

@Temperature 1000 °C,
Time 10800 sec
0.142 - 0.35571 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories MIX-1(1:4) Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.000981 - 0.001962 GPa

@Temperature 1000 °C,
Time 10800 sec
0.142 - 0.2846 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories GUN-135L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.000981 - 0.003924 GPa

@Temperature 1350 °C,
Time 10800 sec
0.142 - 0.5691 ksi

@Temperature 2460 °F,
Time 3.00 hour
Chosun Refractories PAC-160 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.000981 - 0.003924 GPa

@Temperature 1500 °C,
Time 10800 sec
0.142 - 0.5691 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories PAC-160 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved