Polymer Property : Puncture Energy = 9.59 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 13.0 J

@Temperature -40.0 °C
9.59 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ISO 6603-2
Eastman Eastar GN002 Copolyester, Natural  (discontinued **)
Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha..
Puncture Energy 13.0 J

@Temperature -40.0 °C
9.59 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ISO 6603-2
Eastman Eastar GN005 Copolyester, Natural  (discontinued **)
Eastar GN005 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN005 copolyester will not crystallize and thus offers wider processing latitude tha..
Puncture Energy 13.0 J
9.59 ft-lb
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 130 GIT 900116 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, suitable for GIT (gas assisted technology), good surface finishApplication Examples: Chain-saw handles, office chair armrests, of..
Puncture Energy 13.0 J

@Load <=102.3 kg,
Temperature 23.0 °C
9.59 ft-lb

@Load <=225.5 lb,
Temperature 73.4 °F
d.a.m.; ISO 6603-2
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified
PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS.
Puncture Energy 13.0 J
9.59 ft-lb
ISO 6603-2
Lanxess Durethan® BKV 215 901510 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning ..
Puncture Energy 13.0 J
9.59 ft-lb
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 35 HTS 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, very good heat-ageing resistance
Puncture Energy 13.0 J

@Temperature -40.0 °C
9.59 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ISO 6603-2
Eastman Drystar 0113 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Puncture Energy 13.0 - 39.0 J

@Temperature -40.0 - -40.0 °C
9.59 - 28.8 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 7.77 J Grade Count:4
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced