Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 60.0 J @Temperature -30.0 °C |
44.3 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66 PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures |
|||
Puncture Energy | 60.0 J @Temperature -30.0 °C |
44.3 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Apec® 1695 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=158 °CPreprocessingMax. Water content |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Apec® 1745 Polycarbonate Easy to demoldsuitable for superheated steam sterilization up to 143 °C as well as for pharmaceutical applications according to United States Pharmacopeia (USP) XXII Class VIsoftening temperature (.. |
|||
Puncture Energy | 60.0 J @Temperature -30.0 °C |
44.3 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Apec® 1795 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=173°CPreprocessingMax. Water content |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Apec® 1800 Polycarbonate Basic gradesoftening temperature (VST/B 120)=185 °CPreprocessingMax. Water content |
|||
Puncture Energy | 60.0 J @Temperature -30.0 °C |
44.3 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Apec® 1897 Polycarbonate Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=182 °CPreprocessingMax. Water content |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® 2556 Polycarbonate MVR (300 °C/1.2 kg) 14 cm3/10 minEasy releaseGood hydrolysis resistanceInjection moldingAvailable in transparentTranslucent and opaque colorsFood contact gradePreprocessingMax. Water content |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® 2558 Polycarbonate ISO 7391-PC,MR,(,,)-18-9MVR (300 °C/1.2 kg) 14.5 cm3/10 minMedical devicessuitable for ETO and steam sterilization at 121 °CComplies with the requirements of FDA-modified ISO 10993-1 and USP Class.. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® 2656 Polycarbonate ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAv.. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® 2665 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt temp.. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® 2856 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAva.. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® 2867 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt tem.. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® 3103 MAS157 Polycarbonate ISO 7391-PC,EL,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minExtrusionHigh viscosityUV stabilizedAvailable in color code 550115 onlySolid sheetCorrugated sheetPreprocessingMax. Water conte.. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® 3106 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable.. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® 3107 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minGeneral purposeHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpare.. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® 3156 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtru.. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® 6457 Polycarbonate, Flame Retardant Grade MVR (300 °C/1.2 kg) 12.5 cm3/10 minUL 94V-0/3.0 mmUV stabilizedeasy releaseinjection moldingavailable in transparent, translucent and opaque colorsPreprocessingMax. Water content |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® 6717 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-05-9Global gradeFormerly Makrolon DP1-1853MVR (300 °C/1.2 kg) 3.0 cm3/10 minFlame retardantUL 94V-0/2.0 mmHigh viscosityBranchedUV stabilizedEasy releaseInjection molding - Me.. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® DP1-1821* Polycarbonate Developmental productMVR (300 °C/1.2 kg) 6.0 cm3/10 minHigh viscosityUV stabilizedEasy releaseInjection moldingAvailable in colorless transparent onlyPreprocessingMax. Water content |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® LQ3147 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear tints .. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® LTG2623 Polycarbonate PreprocessingMax. Water content |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® Rx2430 Polycarbonate ISO 7391-PC,M,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minMedical devicessuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modified ISO 10993-1 an.. |
|||
Puncture Energy | 60.0 J @Temperature -30.0 °C |
44.3 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® T7855 Polycarbonate, Impact Grade ISO 7391-PC,MPR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPre.. |
|||
Puncture Energy | 60.0 J @Temperature -30.0 °C |
44.3 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® WB1239 Polycarbonate ISO 7391-PC,B,(,,)-05-9Global gradeMVR (300 °C/1.2 kg) 2.5 cm3/10 minBlow moldingHigh viscosityBranchedFood contact qualityExtrusion blow moldingInjection stretch blow moldingAvailable in transpare.. |
|||
Puncture Energy | 60.0 J @Temperature -30.0 °C |
44.3 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® 1248 Polycarbonate, Impact Grade ISO 7391-PC,MP,(,,)-09-9Formerly Makrolon KU1-1248MVR (300 °C/1.2 kg) 7.0 cm3/10 minFood contact qualityMedium viscosityImpact modifiedInjection molding - Melt temperature 280 - 320 °CAvailable in.. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® DP1-1843* Polycarbonate ISO 7391-PC,RL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 9.5 cm3/10 minMedium viscosityUV stabilizedRotomoldingAvailable in transparent and translucent colorsGlobe lightsAs of 1 September 2.. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® LQ3187 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable i.. |
|||
Puncture Energy | 60.0 J @Temperature 23.0 °C |
44.3 ft-lb @Temperature 73.4 °F |
ISO 6603-2 |
Covestro Makrolon® Rx2635 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Med.. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® LQ2687 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9MVR (300 °C/1.2 kg) 12.5 cm3/10 minOptical lensMedium viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear t.. |
|||
Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
Covestro Makrolon® Rx1452 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie.. |