Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 0.463 J | 0.342 ft-lb | ExxonMobil Method |
ExxonMobil LD 143.26 High Clarity Packaging Film Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
Puncture Energy | 0.463 J | 0.342 ft-lb | ExxonMobil Method |
ExxonMobil LDPE LD 143.26 Low Density Polyethylene Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
Puncture Energy | 0.463 J | 0.342 ft-lb | ExxonMobil Method |
ExxonMobil LDPE LD 312.23 Low Density Polyethylene Resin Product Description: LD 312 resins are 4.6% vinyl acetate copolymers for films with good toughness. The comonomer content and low melt index of those resins help produce films which exhibit superior.. |
|||
Puncture Energy | 0.463 J | 0.342 ft-lb | ExxonMobil Method |
ExxonMobil LDPE LD 312.82 Low Density Polyethylene Resin Product Description: LD 312 resins are 4.6% vinyl acetate copolymers for films with good toughness. The comonomer content and low melt index of those resins help produce films which exhibit superior.. |