Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 13.0 J @Temperature -40.0 °C |
9.59 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ISO 6603-2 |
Eastman Eastar GN002 Copolyester, Natural
(discontinued **) Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Puncture Energy | 13.0 J @Temperature -40.0 °C |
9.59 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ISO 6603-2 |
Eastman Eastar GN005 Copolyester, Natural
(discontinued **) Eastar GN005 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN005 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Puncture Energy | 13.0 J | 9.59 ft-lb | Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 130 GIT 900116 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, suitable for GIT (gas assisted technology), good surface finishApplication Examples: Chain-saw handles, office chair armrests, of.. |
|||
Puncture Energy | 13.0 J @Load <=102.3 kg, Temperature 23.0 °C |
9.59 ft-lb @Load <=225.5 lb, Temperature 73.4 °F |
d.a.m.; ISO 6603-2 |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |
|||
Puncture Energy | 13.0 J | 9.59 ft-lb | ISO 6603-2 |
Lanxess Durethan® BKV 215 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning .. |
|||
Puncture Energy | 13.0 J | 9.59 ft-lb | Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 35 HTS 901510 Nylon 6, 35% Glass Fiber PA 6, injection molding grade, 35% glass fibers, very good heat-ageing resistance |
|||
Puncture Energy | 13.0 J @Temperature -40.0 °C |
9.59 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ISO 6603-2 |
Eastman Drystar 0113 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Puncture Energy | 13.0 - 39.0 J @Temperature -40.0 - -40.0 °C |
9.59 - 28.8 ft-lb @Temperature -40.0 - -40.0 °F |
Average value: 7.77 J Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |