Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.73 GPa | 831 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp RFZ42 PA 66 LNP* Thermocomp* RFZ42 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 5.73 GPa | 831 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WFB62 PBT LNP* THERMOCOMP* WFB62 is a compound based on PBT resin containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Low Warpage. |
|||
Flexural Modulus | 5.73 GPa | 831 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp RFZ42 PA 66 (Asia Pacific) LNP* Thermocomp* RFZ42 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass.This data was supplied by SABIC-IP for the Asia Pacific region. |