Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.83 GPa | 700 ksi | ASTM D790 |
Nylene® Norpex® AX20GF , 20% Glass Reinforced Polyphenylene Ether Description: Norpex® AX20GF us a 20% glass fiber reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric.. |
|||
Flexural Modulus | 4.83 GPa | 700 ksi | ASTM D790 |
Oxford Polymers Oxnilon 66-ST-30GF 30% Glass Fiber Reinforced, Impact Modified Nylon 66 for Injection Molding 30% Glass Fiber Reinforced, Impact Modified Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 4.83 GPa | 700 ksi | ASTM D790 |
Niche Polymer PA66GF13BK Nylon 66, 13% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 4.83 GPa | 700 ksi | ASTM D790 |
Niche Polymer PA66GF13N Nylon 66, 13% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 4.83 - 8.96 GPa | 700 - 1300 ksi | Average value: 6.48 GPa Grade Count:15 |
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Flexural Modulus | 4.83 GPa | 700 ksi | ASTM D790 |
PolyOne Edgetek® PF-05GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 4.83 GPa | 700 ksi | ASTM D790 |
Global XNY-577 20% Reinforced Polycarbonate/Polyester Alloy Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 4.83 GPa | 700 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF13 TL10 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: PTFE Lubricant (10%)Features: LubricatedAppearance: Natural ColorInformation .. |
|||
Flexural Modulus | 4.83 GPa | 700 ksi | ASTM D790 |
Techmer ES HiFill® PBT GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.83 GPa | 700 ksi | ASTM D790 |
Clariant Renol PA213G13 Nylon 6, 13% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 4.83 GPa | 700 ksi | Secant at 0.5 Deflection; ASTM D790 |
Applied Composites 8022 Polyester SMC Industry Application: ConstructionProduct Application: Water TreatmentDistinct Features: Ideal for Buried Applications, Construction, High Corrosion Resistance in Waste Water Treatment, Dimensional .. |
|||
Flexural Modulus | >= 4.83 GPa | >= 700 ksi | ASTM D790 |
Buckeye Polymers BP RPP 3009 GKW Polypropylene, Glass Filled Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en.. |
|||
Flexural Modulus | 4.83 GPa | 700 ksi | ASTM D790 |
PolyOne Edgetek® PI-10GF/000 Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 4.83 GPa | 700 ksi | Tangent; ASTM D790 |
Fiberfil® J-60/30/E5 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 4.83 GPa | 700 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GFB20 20% Glass/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead/Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabiliz.. |