Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.455 GPa | 66.0 ksi | |
Dow DOWLEX™ 2507 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2507 Polyethylene resin is a narrow molecular weight distribution copolymer designed for fast injection molding of thin wall lids without warping. It has demonstrated excellent processabili.. |
|||
Flexural Modulus | 0.455 GPa | 66.0 ksi | ASTM D790 |
Quadrant EPP Quicksilver® UHMW-PE Premium Truck Lining (ASTM Product Data Sheet) |