Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.22 GPa | 612 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp DFP22H PC LNP* Lubricomp* DFP22H is a compound based on Polycarbonate containing Glass Fiber and PTFE. Characteristics of this grade are: Internally Lubricated and Healthcare.This data was supplied by SABIC.. |
|||
Flexural Modulus | 4.22 - 12.1 GPa | 612 - 1760 ksi | Average value: 7.10 GPa Grade Count:24 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Flexural Modulus | 4.22 GPa @Thickness 3.20 mm |
612 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2100 PBT+GF10% Description: Injection Molding, PBT+GF10%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Flexural Modulus | 4.22 GPa @Thickness 3.20 mm |
612 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY ER5151RFA PC/ABS Mineral Filler, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High strength, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 14807-96-6Information p.. |
|||
Flexural Modulus | 4.22 GPa | 612 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® VB-3100G PBT/ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 4.22 GPa | 612 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® VB-3100G PBT/ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 4.22 GPa | 612 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX675 PPE+PA6 Noryl GTX* GTX675 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to a.. |
|||
Flexural Modulus | 4.22 GPa | 612 ksi | Resin property; RT; Dry |
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin HexFlow® RTM651 is a one-component modified bismaleimide for resin transfer molding (RTM). Upon heating to 212-248°F, the resin will become a low viscosity homogeneous liquid that has a long pot-l.. |
|||
Flexural Modulus | 4.22 GPa | 612 ksi | ASTM D790 |
Gromax CCP PBT 3010-104 10% Glass Fiber Filled Product Description: PBT glass fiber 10% reinforced injection molding grade.Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent.. |