Mechanical Properties Metric English Comments
Flexural Modulus 4.21 GPa
610 ksi
Tangent; ASTM D790
RheTech Products F43-01A 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Electrical component supportsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 4.21 GPa
610 ksi
Tangent; ASTM D790
RheTech Products F43-01B 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Drip trayFunctional supportsA/C housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 4.21 GPa
610 ksi
ASTM D790
Polymer Resources TP-IM-G15 Polybutylene Terephthalate, 15% Glass Reinforced, Impact Modified
Polybutylene Terephthalate, 15% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Flexural Modulus 4.21 GPa
610 ksi
Tangent; ASTM D790
Fiberfil® PP-60/TC/40/OP WT2595 Polypropylene Homopolymer, 40% Talc Filled, high opacity
Information provided by FIBERFIL Engineered Plastics
Flexural Modulus 4.21 GPa
610 ksi
ASTM D790
M. Holland Company SA500 Styrene Acrylonitrile
High clarityGood processabilityHigh stiffnessApplications: Color concentratesCompounding
Flexural Modulus 4.21 GPa
610 ksi
ASTM D790
Techmer ES Electrafil® NY-3/EC BK PA6