Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.33 - 9.65 GPa | 484 - 1400 ksi | Average value: 7.20 GPa Grade Count:89 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Flexural Modulus | 3.33 GPa | 484 ksi | ASTM D790 |
Lendell Parapet EH-1000 PMMA, Extrusion |
|||
Flexural Modulus | 3.33 GPa @Thickness 3.20 mm |
484 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
Flexural Modulus | 3.33 GPa | 484 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1101 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 3.33 GPa | 484 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1101 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 3.34 GPa | 484 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp TX88477 PU LNP* Thermocomp* TX88447 is a compound based on Polyurethane resin containing proprietary fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 3.33 GPa | 484 ksi | ASTM D790 |
Samyang Trirex® 3025GRU30 Polycarbonate, 30% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electr.. |