Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 22.7 GPa | 3290 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66 LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Heat Stabilized... |
|||
Flexural Modulus | 22.7 GPa | 3290 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66 (Asia Pacific) LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 22.7 GPa | 3290 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA LNP* LUBRICOMP* UCL36S is a compound based on Polyphthalamide resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Heat Stabilized, Electrically Con.. |
|||
Flexural Modulus | 22.7 GPa | 3290 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA (Asia Pacific) LNP* Lubricomp* UCL36S is a compound based on Polyphthalamide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Heat Stabilized, Electrically Cond.. |
|||
Flexural Modulus | 22.7 GPa | 3290 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp LC008 PEEK (Europe-Africa-Middle East) LNP* Thermocomp* LC008 is a compound based on Polyetheretherketone resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 22.7 GPa | 3290 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66 LNP* LUBRICOMP* RCL36 is a compound based on Nylon 66 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wesr Resistant, Electrically Conductive. |