Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.214 GPa | 31.0 ksi | ISO 178/1A |
Radici Heraflex® E 4718 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. Low Modulus, Nominal Shore D/15s 43. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Flexural Modulus | 0.214 GPa | 31.0 ksi | 1% secant; ASTM D790 |
ExxonMobil LD 051.LJ Molding, Extrusion and Compounding Resin
(discontinued **) LD 051.LJ resin is used in Blow molded, squeeze bottles, Pail lids, Closures, and Extruded profiles.Information provided by ExxonMobil Chemical |
|||
Flexural Modulus | 0.214 GPa | 31.0 ksi | ASTM D790 |
Multibase Multi-Flex® D 4000 TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Blow MoldingInformation provided by Multibase |
|||
Flexural Modulus | 0.214 GPa | 31.0 ksi | ASTM D790 |
Multibase Multi-Flamâ„¢ 2903 LDPE Polyethylene Features:Flame RetardantHalogen Content, Low to NoneBlooming, None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingInformation provided by Multibase |
|||
Flexural Modulus | 0.214 GPa | 31.0 ksi | ASTM D790 |
Multibase Multi-Flex® D 5302 ELF Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 0.214 - 0.262 GPa | 31.0 - 38.0 ksi | Average value: 0.236 GPa Grade Count:5 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |
|||
Flexural Modulus | 0.214 GPa | 31.0 ksi | ASTM D790 |
Amco PRIMATOP LDPE 023919 Blow Molding Polyethylene LDPE 023919 features good heat sealing latitude and easy processability. Applications include food contact, squeeze bottles, and non-escr.Former A-Top Polymers product; part of Amco product line sin.. |
|||
Flexural Modulus | 0.214 GPa | 31.0 ksi | ASTM D790 |
Chase Plastics CP Pryme® PE-100LD20M General Purpose Low Density Polyethylene Information provided by Chase Plastics. |