Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
PolyOne Maxxam™ JN-818.S001-1000 Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790 |
Network Polymers NPP 30-2000 TF20 Description: 20% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | |
Protective Coating PC-Rot Terminator® Epoxy Wood Consolidant Description: PC-Rot Terminator® is designed to strengthen decayed or rotted wood. The mixture is a low viscosity liquid that penetrates porous surfaces filling and sealing voids with an epoxy that .. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Europe-Africa-Middle East) 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Polymer Resources NY6-IM1 Nylon 6, Impact Modified Nylon 6, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (.. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
PolyOne Edgetek® AT-000/000 HI5 Natural NA Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
M. Holland Company AB105 ABS Features: Medium Flow, High Impact Resistance, Good StiffnessUses: Household Goods, Packaging Processing Method: Injection MoldingInformation provided by M. Holland. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Techmer ES Luriblend® TPX-PPO/HIPS-02072 BK Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and HomopolymerUL File Number: E157318Information provided by TP Composites,.. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS 8004 UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS 8004 UV MB Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceTPCI# 6816121Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/ABS 1120 B1 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Techmer ES Luriblend® ABS SL2 Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS 8004 Availability: North AmericaForms: PelletsFeatures: General Purpose and High Impact ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Total PSI 830 Polystyrene Polystyrene 830 is a high melt flow, high impact polystyrene specially designed for hard to fill injection molding applications. The high flow 830 material aids production of stress free parts.The m.. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Clariant Renol PA1SP0005 Nylon 66, Impact Modified, Glass Reinforced Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Engineered Plastics EPABS 54 ABS Injection Grade Pellets. GMP # 002. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Aaron Industries AAROLENE® ARPP C 200-3 Polypropylene Compounded Resin AAROLENE® ARPP 200 Series Polypropylene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Aaron Industries AAROLENE® ARPS 100-3 HIPS Black Extrusion Grade Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinFeatures: A high impact Polystyrene, custom colored black, featuring good flow and excellent toughness for all extrusion applications. |
|||
Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
Polymer Resources PPX-SF1 Modified PPO, Structural Foam Grade, Easy Flow
(Unverified Data**) Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Flexural Modulus | 2.07 - 8.10 GPa | 300 - 1170 ksi | Average value: 5.52 GPa Grade Count:29 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Flexural Modulus | >= 2.07 GPa | >= 300 ksi | ASTM D790 |
Buckeye Polymers BP RPP 4008 TR BLK Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |