Mechanical Properties Metric English Comments
Flexural Modulus 0.207 GPa
30.0 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE D 4201 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.207 GPa
30.0 ksi
2% Secant; ASTM D 790
Chevron Phillips 1006 LDPE Injection Molding Resin  (discontinued **)
Resin Type: homopolymerCharacteristics: excellent flexibility, excellent flow, good warping resistance, moderate mold release, moderate ESCRApplications: large housewares, tamper evident snap-on cap..
Flexural Modulus 0.207 GPa
30.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 1550A Polyethylene  (discontinued **)
Injection molding gradeUnless otherwise noted, all tests are run at 23°C and 50% RH. Where required, samples are compression molded per ASTM D1928.Information from manufacturer data sheet.Eastman ..
Flexural Modulus 0.207 GPa
30.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 1550P Polyethylene  (discontinued **)
Injection molding gradeUnless otherwise noted, all tests are run at 23°C and 50% RH. Where required, samples are compression molded per ASTM D1928.Information from manufacturer data sheet.Eastman ..
Flexural Modulus 0.207 GPa
30.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 1830A Polyethylene  (discontinued **)
Polyethylene 1830A is a low density formulation. It is suggested for injection molding applications requiring good stiffness or gloss properties . It us used in applications such as closures.Polyet..
Flexural Modulus 0.207 GPa
30.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 1830E Polyethylene  (discontinued **)
Polyethylene 1830E is a low density formulation. It is suggested for general purpose extrusion applications, such as tubing and blow molding. Polyethylene 1830E meet the requirements of FDA regula..
Flexural Modulus 0.207 GPa
30.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 1870A Polyethylene  (discontinued **)
Polyethylene 1870A is a low density formulation with excellent flow characteristics for injection molding. It is used for such applications as container closures that require stress-crack resistanc..
Flexural Modulus 0.207 GPa
30.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 808A Polyethylene  (discontinued **)
Low density polyethylene 808A is a general-purpose formulation used for injection molding and general-purpose extrusion.Unless otherwise noted, all tests are run at 23°C and 50% RH.Information from..
Flexural Modulus 0.207 GPa
30.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 808P Polyethylene  (discontinued **)
Low density polyethylene 808P is a low density resin designed for applications, such as sugar pouches and freezer wrap, where high coating speeds and good drawdown are required. The combination of ..
Flexural Modulus 0.207 GPa
30.0 ksi
ASTM D790
3M Dyneon™ THV™ 500 Fluorothermoplastic  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf..
Flexural Modulus 0.207 GPa
30.0 ksi
ASTM D790
Multibase Multi-Flex® D 3104-8 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot..
Flexural Modulus 0.207 GPa
30.0 ksi
ASTM D790
Techmer ES HiFill® TPU 0266 A
Availability: North AmericaForms: PelletsFeatures: High Density and High Specific GravityInformation provided by TP Composites, Inc.
Flexural Modulus 0.207 GPa
30.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP763-01 Extruded, Blow Molding and Injection Molding Grade Polyethylene
DescriptionCP 763-01 is an extruded, blow molding, and injection molding grade of low density polyethylene having good processability and heat sealability. ApplicationCP 763-01 meets the specificat..
Flexural Modulus 0.207 GPa
30.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP763-01 Extruded, Blow Molding and Injection Molding Grade Polyethylene
DescriptionCP 763-01 is an extruded, blow molding, and injection molding grade of low density polyethylene having good processability and heat sealability. ApplicationCP 763-01 meets the specificat..
Flexural Modulus 0.207 GPa
30.0 ksi
ASTM D790
Westlake Plastics Clariflex® TFE/VF2/HFP
Clariflex is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoro-propylene, and vinylidene fluoride. Notable properties include light transmission, chemical resistance..
Flexural Modulus 0.207 GPa
30.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP763-01 Extruded, Blow Molding and Injection Molding Grade Polyethylene
DescriptionCP 763-01 is an extruded, blow molding, and injection molding grade of low density polyethylene having good processability and heat sealability. ApplicationCP 763-01 meets the specificat..
Flexural Modulus 0.207 GPa
30.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP763-01 Extruded, Blow Molding and Injection Molding Grade Polyethylene
DescriptionCP 763-01 is an extruded, blow molding, and injection molding grade of low density polyethylene having good processability and heat sealability. ApplicationCP 763-01 meets the specificat..
Flexural Modulus 0.207 GPa
30.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP763-01 Extruded, Blow Molding and Injection Molding Grade Polyethylene
DescriptionCP 763-01 is an extruded, blow molding, and injection molding grade of low density polyethylene having good processability and heat sealability. ApplicationCP 763-01 meets the specificat..
Flexural Modulus 0.207 GPa
30.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP763-01 Extruded, Blow Molding and Injection Molding Grade Polyethylene
DescriptionCP 763-01 is an extruded, blow molding, and injection molding grade of low density polyethylene having good processability and heat sealability. ApplicationCP 763-01 meets the specificat..
Flexural Modulus 0.207 GPa
30.0 ksi
ASTM D790
AdvanSource Biomaterials ChronoFlex® C 75D Biodurable Medical Grade Polyurethane
ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome..
Flexural Modulus 0.207 GPa
30.0 ksi
ASTM D790
Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)  (discontinued **)
Description: PELLETHANE® 2104-65D Polyester based. Excellent oil and chemical resistance. Applications include: Caster wheels, Seals, Gaskets, Animal tags, Hose jacketing, Ski boots, AutomotiveDat..
Flexural Modulus 0.207 GPa
30.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman D4042-P Polyethylene  (discontinued **)
D4042-P is a low density resin designed for applications such as sugar pouches and freezer wrap, where high coating speeds and good drawdown are required. The combination of high melt index and low..
Copyright © lookpolymers.com All Rights Reserved