Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.193 GPa | 28.0 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE A 9502 BLK , 7% Filler Content The moisture content is 0.02%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 0.193 GPa | 28.0 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips KN 230 LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ESCRApplications:Houseware.. |
|||
Flexural Modulus | 0.193 GPa | 28.0 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips KN 230B LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate .. |
|||
Flexural Modulus | 0.193 GPa | 28.0 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips Marlex® 1409 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Excellent Warping Resistance, Excellent Mold Release, Moderate ESCRApplications.. |
|||
Flexural Modulus | 0.193 GPa | 28.0 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman 1390P Polyethylene
(discontinued **) Low-density polyethylene 1390P is used primarily in extrusion-coating applications that require fast line speeds and relatively low coating weights. When compared with other low-density polyethylen.. |
|||
Flexural Modulus | 0.193 GPa | 28.0 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman 808E Polyethylene
(discontinued **) Low density polyethylene 808E is a general-purpose formulation used general-purpose extrusion. Under regulations administered by the US FDA, 808E may lawfully be used as articles or components of a.. |
|||
Flexural Modulus | 0.193 GPa | 28.0 ksi | ASTM D790 |
Multibase Multi-Flex® A 8620 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Thermal Stability, GoodOzone Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automotive Interior PartsCoverings, ProtectiveInformation provide.. |
|||
Flexural Modulus | 0.193 GPa | 28.0 ksi | ASTM D790 |
Multibase Multi-Flex® D 3104 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI.. |
|||
Flexural Modulus | 0.193 GPa | 28.0 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips Marlex® 1412 Injection Molding Resin Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Excellent Warping Resistance, Excellent Mold Release, Moderate ESCRApplications.. |
|||
Flexural Modulus | 0.193 - 0.248 GPa | 28.0 - 36.0 ksi | ASTM D790 |
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |