Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.58 GPa | 229 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers MS 175 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.58 - 3.53 GPa | 229 - 512 ksi | Average value: 3.13 GPa Grade Count:65 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Modulus | 1.58 GPa @Temperature 23.0 °C |
229 ksi @Temperature 73.4 °F |
ASTM D790A |
Ineos H38G-02 Polypropylene Homopolymer This is a polypropylene homopolymer for general purpose injection molding and high speed spinning applications. It is useful for spun bonded nonwovens and partially oriented yarn (POY). This mater.. |
|||
Flexural Modulus | 1.58 GPa | 229 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 2-9000 MA N Polypropylene Copolymer INNOPOL® CS 2-9000 MA N is a high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA N is developed for producing injection molded automotive components.All information provide.. |
|||
Flexural Modulus | 1.58 GPa | 229 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP MX91206 PP LNP* Lubricomp* MX91206 is a compound based on Polypropylene containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 1.58 GPa | 229 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY A3000TXJ ABS LNP* STAT-LOY* A3000TXJ is a product based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives. |
|||
Flexural Modulus | 1.58 GPa | 229 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0855YS ABS, Unreinforced FR Flame-retardant ABS that can be used in the exterior of monitorsInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.58 GPa | 229 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0855YS ABS, Unreinforced FR Flame-retardant ABS that can be used in the exterior of monitorsInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.58 GPa | 229 ksi | ASTM D790 |
Braskem H 201 Fiber Extrusion Polypropylene Applications: Staple fibers for carpets and blankets; continuous filament for ropes, cords and rugs. Information provided by Braskem |
|||
Flexural Modulus | 1.58 GPa | 229 ksi | |
Abatron AboCast 50-11/AboCure 50-1 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/35 ratio. Pot life: 500 g, 240 min. at 25°C(77°F). Exothermic Peak 190°C (375°F). Hardens in 2-24 hours.. |
|||
Flexural Modulus | 1.58 - 3.16 GPa | 229 - 458 ksi | Average value: 2.44 GPa Grade Count:11 |
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max.. |