Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 213 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.47 GPa
213 ksi
Tangent; 1.3 mm/min; ASTM D790
Mytex Polymers AS33LW Polypropylene, Rubber modified, Talc filled, Compounded
Description: AS33LW is a compounded, talc, rubber modified polypropylene for exterior automotive applications. Material has outstanding moldability and excellent balance of high stiffness and good ..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Omni Plastics OmniTuff™ CPP TF20 Copolymer Polypropylene Talc Filled
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
PolyMirae Moplen HP420J BDDP Film Grade Polypropylene
Moplen HP420J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP420J is a homopolymer particularly suitable for BOPP (Tender) fi..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
PolyMirae Moplen HP550K Stretch/Yarn, Monofilament Grade Polypropylene
Moplen HP550K is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP550K is a homopolymer suitable for rope, tape, yarn, monofilament..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
PolyMirae Moplen HP552R Fiber (Staple/BCF/CF) Grade Polypropylene
Moplen HP552R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP552R is a homopolymer typically used by customers in high speed p..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
PolyMirae Moplen HP553P Fiber (Staple) Grade Polypropylene
Moplen HP553P is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP553P is a homopolymer typically used by customers in high speed p..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
PolyMirae Moplen HP557G Stretch Grade Polypropylene
Moplen HP557G is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP557G is a homopolymer suitable for high strength rope, container ..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
PolyMirae Moplen HP562S Fiber (Spunbond) Grade Polypropylene
Moplen HP562S is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562S is a homopolymer particularly suitable f..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
PolyMirae Moplen EP540R Injection Molding Grade Polypropylene
Moplen EP540R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP540R is a block copolymer particularly suitable for injection..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Hyosung Topilene B200 PP
B200 Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:StiffnessFormabilityInformation provided by Hyosung Corporation
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Hyosung Topilene B200P PP
B200P Applications: Industrial pipesCharacteristics: Chemical resistanceInformation provided by Hyosung Corporation
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Hyosung Topilene B201Y PP
B201Y Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:Low smellFormabilityInformation provided by Hyosung Corporation
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Hyosung Topilene F400 PP
F400 Film Grade HomopolymerApplications: OPPCharacteristics:ProcessabilityTransparencyInformation provided by Hyosung Corporation
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Hyosung Topilene HJ340 PP
HJ340 Impact CopolymerApplications:Corrugated sheetThick board (tank, etc…)Characteristics:High impactHigh stiffnessLow warpageInformation provided by Hyosung Corporation
Flexural Modulus 1.47 GPa
213 ksi
1% Secant; ASTM D790
Flint Hills P4C6Z-022 Homopolymer Polypropylene
Homopolymer, UL certified, and FDA compliant.Features: Controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by Flint Hills Res..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Hyosung Topilene J742 PP
J742 Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corporat..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Hyosung Topilene J842 PP
J842 Injection Impact CopolymerApplications: Very large articles:Washing M/C partsIndustrial applianceCharacteristics:High flowabilityHigh stiffnessInformation provided by Hyosung Corporation
Flexural Modulus 1.47 GPa

@Thickness 3.20 mm
213 ksi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUCEL HI520 POM+Rubber, High Impact
Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical
Flexural Modulus 1.47 GPa
213 ksi
ASTM D760
LG Chemical SEETEC H5300 Polypropylene, Homopolymer
Features: Seetec H5300 is designed for the extrusion of textile yarn and monofilaments. This grade is characterized by good processability and stretchability. SEETEC H5300 meets the FDA requirement ..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D760
LG Chemical SEETEC H7411 Polypropylene, Homopolymer
Features: Seetec H7411 is designed for the extrusion of continuous filament (CF) and staple fibers. This grade is characterized by high tenacity from narrow molecular weight distribution (MWD) and U..
Flexural Modulus 1.47 GPa
213 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-LOY 93000LTH Acrylic
LNP* STAT-LOY* 93000LTH is a compound based on Acrylic resin. Added features of this material include: Antistatic, Transparent and Formulation Locked.
Flexural Modulus 1.47 GPa
213 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS
LNP* STAT-LOY A3000T is a compound based on ABS. Added features of this grade include: Antistatic, Clear.
Flexural Modulus 1.47 GPa

@Thickness 3.20 mm
213 ksi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SH 2157 High Impact Polystyrene
Characteristics Excellent ESCR properties Good formability Processing ExtrusionApplications Refrigerator door and cabinet liners Dairy containers Ice cream cups, plates and bowlsMaterial Status: ..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
SCG Chemicals EL-Leneâ„¢ H6430BM High Density Polyethylene Blow Molding
Key Characteristics:Excellent stiffnessGood processabilityOdorlessSafe for food contactGood printabilityRecommended Applications:Bottles for drinking water, fruit juice, soft drink, milkAutomotive p..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
SCG Chemicals EL-Leneâ„¢ H6670B High Density Polyethylene Film
Key Characteristics:High flowExcellent processabilityHigh stiffnessOdorlessSafe for food contactGood printabilityRecommended Applications: Bottles for drinking water, fruit juice, soft drink, milkI..
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman.
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Tipco Tipcolene® FPC 10 PPC - 10% Calcium Carbonate Reinforced Polypropylene Copolymer
10% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman.
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman.
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman.
Copyright © lookpolymers.com All Rights Reserved