Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.207 GPa | 175.1 ksi | Tangent-Method 1; ASTM D790 |
Ineos T50-4400 HDPE Ineos T50-4400 is a high-flow high density polyethylene copolymer intended for injection molding of thin wall containers. This material will allow for cycle time reduction while still imparting rea.. |
|||
Flexural Modulus | 1.207 GPa | 175.1 ksi | Tangent; ASTM D 790 |
Ineos J50-1000-178 HDPE A high density polyethylene copolymer intended for the injection molding of closures for beverages. Because of its high purity and excellent organoleptic properties, this grade is certified as low .. |
|||
Flexural Modulus | 1.207 GPa | 175.1 ksi | Tangent-Method 1; ASTM D790 |
Ineos J50-1000-181 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin c.. |
|||
Flexural Modulus | 1.207 GPa | 175.1 ksi | Tangent-Method 1; ASTM D790 |
Ineos J50-1000-187 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin con.. |