Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
PolyOne Nymax™ GF 600 A 44 Black 13 Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
Oxford Polymers 40GF 40% Glass Fiber Reinforced Polyphenylene Sulfide 40% Glass Fiber Reinforced Polyphenylene SulfideInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
Oxford Polymers PPS-40GF PPS, 40% Glass Fiber Reinforced Product Description: Glass Fiber (40% Reinforced), Polyphenylene sulfide injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAppearance: Natural or BlackInformation p.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
Quantum Composites QC-8777 41% Glass Fiber Reinforced Polyester Hybrid SMC QC-8777 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength, corrosion resistance and temperature.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | Conditioned; ASTM D790 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-8930 HS Polyphthalamide (PPA), 30% Glass Fiber Amodel® A-8930 HS is a 30% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 126F10 Nylon 6, 50% Glass Fiber SAXAMID 126F10 is a polyamide 6 injection-molding-grade reinforced with 50% glass fibers.Information provided by SAX Polymers |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
Chem Polymer Durlex 740-10 GB PBT, 40% Short Glass Fiber, 10% Glass Bead Reinforced A 40% short glass fiber, 10% glass bead reinforced PBT, offering a combination of tensile strength, warpage control and dimensional stability for close tolerance applications.Data provided by the ma.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 617 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.55% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-6135 NL Polyphthalamide (PPA), 35% Glass Fiber Reinforcement
(discontin Amodel A-6135 NL polyphthalamide (PPA), a 35% glass reinforced, high-glow, non-lubricated, hot-water moldable resin specially designed for laser welding. The black version is a laser absorber, and t.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | 5 mm/min; ISO 178 |
Gromax CFG45-RN13N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |