Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.05 GPa | 152 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PQ 82 N Polypropylene with improved impact strength PP impact modified. General application in all industry branches. Delivered in natural mode and in the full RAL color scale. For injection molding.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
PolyOne Maxxam™ FR PP FR 7B31 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Flexural Modulus | >= 1.05 GPa | >= 152 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1365S (H22S) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | >= 1.05 GPa | >= 152 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 4215M (EP1X35F) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | >= 1.05 GPa | >= 152 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 8332C (EPD60R) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
SABIC BM1052 High Density Polyethylene for Blow Molding Product Description: BM1052 grade is a high molecular weight High Density Polyethylene copolymer with broad molecular weight distribution. It has excellent processability and exhibits very high im.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | 1% Secant; ASTM D790 |
Flint Hills P5M6K-048 Random Copolymer Polypropylene Random copolymer, FDA compliant.Features: Clarified (50 mil plaque haze 10%), antistat, and controlled rheology.Applications: Injection molding: high clarity parts, medical parts, and good organole.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PRB 4215 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
Iran Petrochemical (PCC) 5218EA High Density Polyethylene HD-5218EA is a high density polyethylene copolymers containing butane-1 as the comonomer with narrow molecular weight distribution, suitable for thin wall injection application. It has been designed.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Iran Petrochemical (PCC) Moplen EP1 X 35 AF Polypropylene Moplen EP1 X 35 AF is a slightly modified random copolymer for the production of cast and water-quenched blown film. It is formulated with a slip and antiblock package and exhibits excellent antist.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D760-66 |
Micropol Microlin ML27 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | |
Kraton® G1652 + PP blend (10/90) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
MRC Polymers MAXTELâ„¢ 600-BK TPO, Black For automotive exterior applications. Excellent process ability and dimensional stability.Unfilled TPOAvailable in black and gray onlyCan be UV StabilizedInternal and external lubricants can be add.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178-1975 |
SIDPEC EGYPTENE® HD 5218 EA HDPE Injection Molding Applications:House waresThin-walled food containersPET bottle base cupInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | At 2 mm/min; ISO 178 |
Borealis Daplen™ EE040AE TPO Compound Daplen EE040AE is an elastomer modified polypropylene compound intended for injection molding. Daplen EE040AE is a material with excellent impact /stiffness ratio. Thanks to its low thermal expansi.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PE HD LITEN® FB 29 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® MB 720 Polypropylene Impact Copolymer Impact copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® MT 825 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® MT 950 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 527-2 |
Total PPC 9712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9712 is heterophasic copolymer. PPC 9712 is characterized by excellent impact resistance and antistatic properties and has been formulated to allow faster cycling through early de.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® GB 608 Polypropylene Impact Copolymer Made for injection molding applications. Slip and antiblocking agent stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® MT 812 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Chengdu Polyster H9275Y Thermoplastic Polyether-ester Elastomer (TPEE) High modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent heat-ageing resistance and toughness. Applications requiring high strength, high toughness and good .. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | 1.0 in/min; 0.125" thickness; ASTM D-790 |
Chevron Phillips K-Resin® XK44 SBC K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:Thermoformed clam shell packagingThermoformed blister packsThermoformed medical traysBlow molded productsFeatures:Good clarityGood stiffnessGo.. |
|||
Flexural Modulus | 1.05 GPa @Temperature 23.0 °C |
152 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® FN718 NC010A Nylon 66 Zytel® FN718 NC010A is a flexible, plasticizer free modified polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
Carmel Olefins CAPILENE® QT 73 AV Propylene Random Copolymer Description: CAPILENE® QT 73 AV is a high melt flow rate, controlled rheology polypropylene random copolymer for injection molding of clear articles. CAPILENE® QT 73 AV is clarified with antista.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
Carmel Olefins CAPILENE® QW 73 AV Propylene Random Copolymer Description: CAPILENE® QW 73 AV is a high melt flow rate, controlled rheology polypropylene random copolymer for injection molding of clear articles. CAPILENE® QW 73 AV is clarified with antista.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
Carmel Olefins CAPILENE® QU 73 AV Propylene Random Copolymer Description: CAPILENE® QU 73 AV is a high melt flow rate, controlled rheology polypropylene random copolymer for injection molding of clear articles. CAPILENE® QU 73 AV is clarified with antista.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, DAM Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, Conditioned Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |