Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
Multibase Multi-Pro® 2513 C Whirlpool White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
RheTech Products FRP255-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
RheTech Products P250-00 Polypropylene Copolymer, Natural Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
RheTech Products P250-247 Polypropylene Copolymer, UV Stabilized, Black Applications: Center consolesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
RheTech Products P251-00 Polypropylene Copolymer, Natural Applications: Fuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
RheTech Products P252-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
RheTech Products P256-00 Polypropylene Copolymer, Natural Applications: Door/trunk scuffUnderhood componentsSplash shieldsElectrical enclosuresInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
Ravago Manufacturing Americas Echo® RPPC 20/6 BK Polypropylene Copolymer Available in North America Recycled Content: Yes Features: CopolymerColor: Black Form: Pellets Information provided by Ravago |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
Formosa Plastics Formolene® HL4506 Blow Molding HDPE
(discontinued **) Extra High Molecular Weight Hexene CopolymerApplications: Multi-layer fuel tanks, mono-layer fuel tanks, industrial bulk containers (IBC)Formolene HL4506 is intended for large part blow molding appl.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | 1% Secant, 0.05 in/min; ASTM D790 |
LyondellBasell Pro-faxâ„¢ SR257M Polypropylene Copolymer Description: Pro-faxâ„¢ SR257M clarified polypropylene random copolymer resin has excellent see-through and contact clarity. This resin offers source reduction potential in blow molding and extru.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | 1% Secant at 0.05 in/min; ASTM D790A |
Ineos R05C-00 Polypropylene Random Copolymer Random copolymer R05C-00 is an antistatic, clarified polypropylene random copolymer produced by a unique catalyst technology. It is designed as a high gloss resin and exhibits good stiffness and imp.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF30 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation p.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
Techmer ES Plastiblend® PA6 GF30 RM BK Nylon 6 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
Techmer ES HiFill FR® PP CO E FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant and CopolymerProcessing Method: ExtrudedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de.. |
|||
Flexural Modulus | 1.03 GPa @Strain 2.00 % |
150 ksi @Strain 2.00 % |
ASTM D790 |
Total HDPE XT10 N High Density Polyethylene - Pipe Resin Polyethylene: High molecular weight, bimodal pipe resin.Characteristics:Outstanding high temperature creep rupture strengthExceptional slow crack growth resistanceExcellent resistance to rapid crac.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | |
TriStar TriSteel AC Metal Backed PTFE Bearing System Ultraflon 601 (AC) POM lined metal backed bearing system, boundary lubrication required, high PV. Ultraflon 601 POM Liner is a lubricant enhanced acetal material for use in lubricated or unlubricate.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | |
TriStar TriSteel AT Metal Backed PTFE Bearing System Ultraflon 601T (AT) POM bronze with PTFE, lined metal back bearing system, high PV, self lube, high speed. This liner will run with zero lubrication required. Most commonly used in clip bearings, li.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 2510A Injection Applications Polypropylene Impact Copolymer with Nucleating, Antistat AdditivesApplications: Closures, housewares, small appliances, battery cases and lids.Formolene 2510A is a medium impact copolymer of polypropylene charact.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 3335E Random Copolymer Polypropylene Random Copolymer for Clear Storage Boxes, Pill Vials and Containers Formolene® 3335E is a high melt flow random copolymer with fast cycle time and easy mold release. It is designed for injection mo.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
A. Schulman PP 1817-01 Polypropylene Utility Grade Random Co-Polymer DescriptionPolypropylene PP 1817-01 is a utility grade random co-polymer which can be used for general purpose injection molding, extrusion, or blow molding applications. It does not have a gel spe.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ AA45-004 Blow Molding Resin Product Description: AA45-004 is a blow molding high density polyethylene copolymer offering exceptional stress cracking resistance and impact performance.Availability: Latin America, North America .. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | 1.3 mm/min, 1% Secant; ASTM D790 |
Amco PRIMATOP PP CO 008NB Impact Polypropylene Copolymer PP CO 008 NB features an excellent balance of toughness and stiffness. Applications include blow molded bottles and containers, blown and cast film applications, and profile extrusions.Former A-Top .. |
|||
Flexural Modulus | 1.03 - 1.72 GPa | 150 - 250 ksi | ASTM D790 |
Alcoa KAMA 3202 Freezer Modified High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableColors availa.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | 1% Secant; ASTM D790 |
ExxonMobil HD 8760.29 Rotational Molding Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ AG45-004 Blow Molding Resin
(discontinued **) AG45-004 is a blow molding high density polyethylene which offers exceptional stress crack resistance and impact performance. It contains an antistat which permits this resin to be used in all food.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D 790 |
Total XT10 N Natural HDPE, pipe Applications: Potable water, industrial and mining, sewer and sewer relining, gas and oil gathering, general pipe relining, pipe coatingInformation provided provided by Total Petrochemicals.Total Pe.. |
|||
Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
PolyOne Edgetek® UR-20GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |