Flexural Modulus 0.931 GPa
135 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Pro® 3011 CHI Grey 29% Filler Content Polypropylene
Data provided by Multibase.
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
Multibase Multi-Pro® 3011 CHI Polypropylene
Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Flexural Modulus 0.931 GPa
135 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers NPP 20-0202
Description: Random Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Flexural Modulus 0.931 GPa
135 ksi
Test Method I, Procedure B (chs speed 0.05 in/min), 1 % Secant; ASTM D790
Network Polymers NPP 25-0202 C
Description: Copolymer Polypropylene, Clarified RandomInformation provided by Network Polymers Inc.
Flexural Modulus 0.931 GPa
135 ksi
2% Secant; ASTM D 790
Chevron Phillips HiD® 9075 HDPE Injection Molding Resin  (discontinued **)
Resin Type: linear copolymer; ASTM D3350 Classification 335540A; ASTM D4976 Classification: PE 235, A 54607Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, e..
Flexural Modulus 0.930 GPa
135 ksi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Modulus 0.931 GPa
135 ksi
Procedure A; ASTM D790
M. Holland Company CP503 Polypropylene Impact Copolymer
Impact copolymerGood impact resistanceLow temperature impact resistanceApplications: Compounding
Flexural Modulus 0.932 GPa
135 ksi
ASTM D790
Hyosung Topilene R530 PP
R530 Random CopolymerApplications: EBMCharacteristics: Transparency USP Class VI certifiedInformation provided by Hyosung Corporation
Flexural Modulus 0.932 GPa
135 ksi
ASTM D790
Hyosung Topilene R530A PP
R530A Random CopolymerApplications: ISBMCharacteristics: Transparency USP Class VI certifiedInformation provided by Hyosung Corporation
Flexural Modulus 0.931 GPa
135 ksi
1.3 mm/min; ASTM D790
ICO Polymers ICORENEâ„¢ 195-1336 LMDPE Rotational Molding Resin
Description: ICORENE 195-1336 is a compounded linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and sti..
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene
DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 0.930 GPa
135 ksi
880 min.; ASTM D790
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene
DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman.
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene
DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 0.930 GPa
135 ksi
880 min.; ASTM D790
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene
DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman.
Flexural Modulus 0.930 GPa
135 ksi
ASTM D790
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene
DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene
DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 0.930 GPa
135 ksi
880 min.; ASTM D790
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene
DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman.
Flexural Modulus 0.930 GPa
135 ksi
ASTM D790
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene
DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
Westlake Plastics Kynar® PVDF CN-P Polyvinylidene Fluoride (conductive)
Carbon-powder-filled, thermally stable, conductive material with consistent resistivities
Flexural Modulus 0.930 GPa
135 ksi
880 min.; ASTM D790
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene
DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman.
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene
DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
CPC - Vycom FLAMETEC™ CP5 Fire Retardant Polypropylene (FRPP)
Flametec™ CP5 was formulated to meet the SEMI S93 specification for fire safety in clean room applications. CP5 meets UL 94 V-0 fire classification and is extruded for gauge and dimensional consist..
Flexural Modulus 0.931 GPa
135 ksi
CMW® ELKONITE® 7065 Infiltrated Molybdenum Silver contact material ASTM B662 Table 1, Class A1
For arcing electrical contactsInformation provided by CMW Inc.
Flexural Modulus 0.930 GPa
135 ksi
ASTM D790
Ashley Polymers Ashlene® TD925H Nylon 12
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption, with UV and he..
Flexural Modulus 0.931 GPa
135 ksi
0.05 in/min, 1% Secant; ASTM D790
Amco PRIMATOP PP CO 350-40 Polypropylene Copolymer
PP CO 350-40 features impact resistance and low temperature stiffness. Applications include injection molding and containers.Former A-Top Polymers product; part of Amco product line since 2013.
Flexural Modulus 0.930 GPa
135 ksi
ASTM D790
ExxonMobil Escorene® HD-8761 LHDPE Rotational Molding Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.HD-8700 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8761 is fully formula..
Flexural Modulus 0.930 GPa
135 ksi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Modulus 0.930 GPa
135 ksi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 16% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Modulus 0.931 GPa
135 ksi
0.05 in/min, 1% secant; ASTM D-790A
Braskem TI6350WV High Impact Copolymer Polypropylene
Description: Superior low temperature impact, nucleated, antistatic.Applications: Suggested uses include furniture, toys, compounding.Process: Injection Molding.This resin meets the requirements for..
Flexural Modulus 0.931 GPa
135 ksi
2% Secant-Method 1; ASTM D790
Ineos HP50-25-153 HDPE
A high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which requiring excellent environmental stress crack resistance (ESCR)...
Copyright © lookpolymers.com All Rights Reserved