Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.196 - 2.55 GPa | 28.4 - 370 ksi | Average value: 2.06 GPa Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Flexural Modulus | 2.24 - 2.55 GPa | 325 - 370 ksi | ASTM D790 |
Alcoa KAMA 4100 Prime APET
(discontinued **) CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Available in clear,.. |
|||
Flexural Modulus | 2.24 - 2.55 GPa | 325 - 370 ksi | ASTM D790 |
Alcoa KAMA 4200 RPET
(discontinued **) CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Up to 100% recycled.. |
|||
Flexural Modulus | 2.24 - 2.55 GPa | 325 - 370 ksi | ASTM D790 |
Alcoa KAMA Petwich-PET 4300 Petwich-PET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Recycled contentSi.. |
|||
Flexural Modulus | 2.24 - 2.55 GPa | 325 - 370 ksi | ASTM D790 |
Alcoa KAMA 4203 Impact Modified RPET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Silicone coating a.. |
|||
Flexural Modulus | 2.41 - 2.55 GPa | 350 - 370 ksi | ASTM D790 |
Alcoa KAMA SealPET™ 4205 RF Sealable RPET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Silicone coating a.. |
|||
Flexural Modulus | 2.41 - 2.55 GPa | 350 - 370 ksi | ASTM D790 |
Alcoa KAMA 4223 Impact Modified RPET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 50”Silicone coatingCl.. |