Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.62 - 16.2 GPa | 1250 - 2350 ksi | Average value: 12.5 GPa Grade Count:17 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Flexural Modulus | 6.55 - 16.2 GPa | 950 - 2350 ksi | Average value: 12.3 GPa Grade Count:28 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Flexural Modulus | 16.2 - 16.2 GPa @Temperature 115 - 115 °C |
2350 - 2350 ksi @Temperature 239 - 239 °F |
Average value: 9.03 GPa Grade Count:1 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |
|||
Flexural Modulus | 4.12 - 16.2 GPa | 597 - 2350 ksi | Average value: 8.50 GPa Grade Count:44 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |