Mechanical Properties Metric English Comments
Flexural Modulus 6.84 - 10.8 GPa
992 - 1570 ksi
Average value: 9.34 GPa Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe..
Flexural Modulus 3.10 - 10.8 GPa

@Temperature -40.0 - 121 °C
450 - 1570 ksi

@Temperature -40.0 - 250 °F
Average value: 5.75 GPa Grade Count:11
Overview of materials for Nylon 66, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Flexural Modulus 10.2 - 10.8 GPa
1480 - 1570 ksi
ASTM D790M
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure
DescriptionNanoTool produces strong, stiff, high temperature resistant composite parts on conventional stereolithography machines. This third generation of Somos® ProtoComposite materials is heavi..
Flexural Modulus 9.00 - 10.8 GPa
1310 - 1570 ksi
Average value: 9.67 GPa Grade Count:3
Overview of materials for Epoxy, Cast, Metal Filled