Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.88 GPa | 1430 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WF007 PBT LNP THERMOCOMP WF007 is a compound based on PBT resin containing 35% Glass Fiber. |
|||
Flexural Modulus | 9.88 GPa | 1430 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp WF007 PET/PBT LNP Thermocomp WF-1007 BK8-114 is a compound based on PET/PBT resin containing glass fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 9.88 GPa | 1430 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RV007ESS PA 66 (Europe-Africa-Middle East) LNP VERTON* RF-7007 EM HS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 9.88 GPa | 1430 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RX06479 PA 66 (Asia Pacific) LNP VERTON* RX06479 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 9.88 GPa | 1430 ksi | ISO 178 |
Polyplastics Duranex® HN7330 Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 9.88 GPa | 1430 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RV007ES PA 66 LNP VERTON* RV007ES is a compound based on Nylon 66 resin containing 35% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Flexural Modulus | 9.88 GPa | 1430 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RX06479 PA 66 LNP VERTON* RX06479 is a compound based on Nylon 66 resin containing 35% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural |
|||
Flexural Modulus | 9.88 GPa | 1430 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RF-7007 EM HS PA 66 (Asia Pacific) LNP VERTON* RF-7007 EM HS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |