Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.31 GPa | 1210 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP ZF006 PPE+PS LNP* THERMOCOMP* ZF006 is a compound based on PPE+PS resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 8.31 GPa | 1210 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP 40% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
Flexural Modulus | 8.31 GPa | 1210 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Asia Pacific) 40% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
Flexural Modulus | 8.31 GPa | 1210 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp LF004 PEEK LNP THERMOCOMP* LF004 is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |