Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.58 GPa | 1100 ksi | Tangent; ASTM D790 |
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Oxford Polymers Oxnilon 66-33GF 33% Glass Fiber Filled Nylon 66 for Injection Molding 33% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2040MGHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Flexural Modulus | 7.58 - 31.0 GPa | 1100 - 4500 ksi | Average value: 17.3 GPa Grade Count:11 |
Overview of materials for PEKK, Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | Conditioned; ASTM D790 |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Greene Tweed Arlon® 1160 PEEK, Glass Filled Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Techmer ES HiFill® ABS GF30 A1 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF35 L UV 35% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KF004AL Acetal Homopoly (Asia Pacific) LNP* Thermocomp* KF004AL is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Techmer ES Electrablend® PA6 04001 FR MB Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel FiberAdditive: LubricatedFeatures: Electromagnetic Shielding (EMI), Lubricated, Flame Retardant and Radio Frequen.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Aaron Industries AAROPRENE® GFPC 5030 Glass Filled Polycarbonate AAROPRENE® GFPC 5000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |