Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.52 GPa | 1090 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
Flexural Modulus | 7.52 GPa | 1090 ksi | ASTM D790 |
Covestro Petlon® DP3-1039 Semi-Crystalline PET, 35% Glass Fiber
(discontinued **) Characteristics: Impact Modified: Good Strength and ToughnessApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperature: 495-530°F, Mold Tempe.. |
|||
Flexural Modulus | 7.52 GPa | 1090 ksi | ASTM D790 |
Ravago Manufacturing Americas Enviramid™ N1335HL BK Nylon 6/6 Available in North America Filler: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedContains Recycled ContentRoHS Compl.. |
|||
Flexural Modulus | 7.52 GPa | 1090 ksi | ASTM D790 |
Ravago Manufacturing Americas Enviramid™ N2335HL BK Nylon 6 Available in North America Filler: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedContains Recycled ContentRoHS Compl.. |
|||
Flexural Modulus | 7.52 GPa | 1090 ksi | ASTM D790 |
LNP Lubricomp® EFL-4034 LE BK8-065 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued ** Features: Low Extractables, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
Flexural Modulus | 7.52 GPa | 1090 ksi | ASTM D790 |
Solvay Technyl® A20V25 25% Glass Filled, V-0 Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Flexural Modulus | 7.52 GPa | 1090 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP D351 PC (Asia Pacific) LNP* Thermocomp* D351 (experimental grade name as EXTC8143) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus,.. |
|||
Flexural Modulus | 7.52 GPa | 1090 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 2F006 ETFE LNP* THERMOCOMP* 2F006 is a compound based on ETFE containing 30% Glass Fiber. |
|||
Flexural Modulus | 7.52 GPa | 1090 ksi | ASTM D790 |
PlastxWorld Veroplas PB3300 Nylon 66 30% glass filled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Flexural Modulus | 7.52 GPa @Thickness 3.17 mm |
1090 ksi @Thickness 0.125 in |
ASTM D790 |
Polyram PB330I8 Nylon 6, 40% Mineral/Glass Filled Heat Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 7.52 GPa | 1090 ksi | ASTM D790 |
PlastxWorld Veroplas PA3300 Nylon 6 general purpose, 30% glass filled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Flexural Modulus | 7.52 - 14.5 GPa | 1090 - 2100 ksi | Average value: 10.7 GPa Grade Count:10 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |