Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.29 GPa | 912 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp RFZ71S PA 66 LNP* Thermocomp* RFZ71S is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 6.29 GPa | 912 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp RFZ71S PA 66 (Asia Pacific) LNP* Thermocomp* RFZ71S is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 6.29 GPa | 912 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MF006AL PP LNP* THERMOCOMP* MF006AL is a compound based on Polypropylene resin containing 30% Glass Fiber. Characteristics of this grade are: Low Extractable. |
|||
Flexural Modulus | 6.29 GPa | 913 ksi | 5 lb Core, 6 hrs @ 220°F, Vacuum Bag |
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive Aroply™ 250 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported knitted nylon carrier. Cured adhe.. |