Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.96 GPa | 864 ksi | ASTM D790 |
PolyOne Stat-Tech™ PI-05CF/000R Black Polyether Imide (PEI) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Flexural Modulus | 5.96 GPa | 864 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PS+PA GR 20%. Higher stiffness of 800000 psi (4000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: valves. |
|||
Flexural Modulus | 5.96 GPa | 864 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PS+PA (Asia Pacific) GR 20%. Higher stiffness of 800000 psi (4000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: valves. |
|||
Flexural Modulus | 5.96 GPa | 865 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR20 IM10 Glass Reinforced/Impact Modified Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |