Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.499 GPa | 797.5 ksi | ASTM D790 |
Styron EMERGEâ„¢ 8702 Polycarbonate EMERGEâ„¢ PC 8702 advanced resin is an ignition-resistant, 20% glass reinforced, polycarbonate resin. This resin contains no bromide, chloride, or phosphate additives. It is a medium flow PC re.. |
|||
Flexural Modulus | 5.499 GPa | 797.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437G40CL Glass Reinforced Coupled |
|||
Flexural Modulus | 5.499 GPa | 797.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334G30CL Glass Reinforced Coupled |
|||
Flexural Modulus | 5.499 GPa | 797.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336G30CL Glass Reinforced Coupled |