Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.394 GPa | 782.3 ksi | ASTM D790 |
Kolon KOPET® KP133G15BL G/F Reinforced Polyester Compound Resin (PET) Dimensionally stable, high elastic, high flowApplications: Ink CartridgeInformation provided by API-Kolon. |
|||
Flexural Modulus | 5.394 GPa | 782.3 ksi | ASTM D790 |
Kolon SPESIN® KP213G15BL Glass Fiber Reinforced PBT Compound Resin b>Characteristics: G/F 15% reinforced, BLACKApplications: Impeller housingsInformation provided by API-Kolon. |
|||
Flexural Modulus | 5.394 GPa | 782.3 ksi | ASTM D790 |
Kolon SPESIN® KP213G15SIBL Glass Fiber Reinforced PBT Compound Resin G/F 15%, high toughness, excellent surfaceApplications: Various types of housingsInformation provided by API-Kolon. |