Polymer Property : Flexural Modulus = 4.58 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.58 GPa
664 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® NX07353 PC+ABS (Asia Pacific)
Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications.
Flexural Modulus 4.58 GPa
664 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® C7230P PC+ABS (Asia Pacific)
Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications.
Flexural Modulus 4.58 GPa
664 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP MX06404 PP
LNP LUBRICOMP* MX06404 is a compound based on Polypropylene resin containing 20% Glass Fiber and 15% PTFE. Added features of this material include: Heat Stabilized, Low Extractable, Wear Resistant...
Flexural Modulus 4.58 GPa
664 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP RF002 PA 66
LNP THERMOCOMP* RF002 is a compound based on Nylon 66 resin containing 10% Glass Fiber.
Flexural Modulus 4.58 GPa
664 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOTUF WF003I Polyester, TP
LNP THERMOTUF* WF003I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.