Mechanical Properties Metric English Comments
Flexural Modulus 30.0 GPa
4350 ksi
ASTM D790
Owens Corning Glass Fiber Reinforced Epoxy (Filament Wound), 80 wt.% glass
Epoxies are highly resistant to water, alkalis and organic solvents. Although standard epoxies have only a fair resistance to acids and oxidizing agents, they can be formulated for better resistance..
Flexural Modulus 30.0 GPa

@Temperature 23.0 °C
4350 ksi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
Flexural Modulus 30.0 GPa
4350 ksi
Lehmann & Voss LUVOCOM® 1105-7290 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Flexural Modulus 30.0 GPa
4350 ksi
Lehmann & Voss LUVOCOM® 1301-0825 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
Flexural Modulus 30.0 GPa
4350 ksi
ASTM D790
Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite