Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.59 GPa | 520 ksi | Tangent; ASTM D790 |
RheTech Products F36-01 35% Mica Reinforced Polypropylene Copolymer, Black Applications: Cowl screensHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | Tangent; ASTM D790 |
RheTech Products G20P100-01UV 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: Rigid exterior componentsHousingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.59 GPa | 521 ksi | ASTM D790 |
PolyOne Maxxam™ PPH-20G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 3.59 GPa | 521 ksi | tangent; ASTM D790 |
S&E Specialty Polymers TufFill™ 5000-SN4 PP, Flame Retardant Application: A No Bloom, UL 94 V-0 Polypropylene Compound TufFill™ 5000SN series is a specially engineered, low bloom, flame retardant polypropylene compound designed with halogen based technology... |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Oxford Polymers 25GB-5GF-IM Polybutylene Terephthalate (PBT), Impact Modified/ Glass Beads Polybutylene Terephthalate (PBT), Impact Modified/ Glass BeadsInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Oxford Polymers PEEK 450-INJ-Black PEEK Product Description: Polyetheretherketone, general purpose injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon black Special Characteristics: Precol.. |
|||
Flexural Modulus | 3.59 GPa | 521 ksi | ASTM D792 |
PTS PPE/Nylon Alloy 10% Glass Filled Information provided by PTS LLC. |
|||
Flexural Modulus | 3.59 - 29.0 GPa | 520 - 4210 ksi | Average value: 11.7 GPa Grade Count:50 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | Tangent; ASTM D790 |
Fiberfil® PP-60/TC/20/VO/ND Polypropylene Homopolymer, 20% Talc Filled, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Global GAB-105 5% Glass Reinforced ABS Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Global MPP-120-C 20% Mica Reinforced Polypropylene Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Techmer ES Electrablend® PC 04006 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Techmer ES Electrablend® PEI 04001 MB Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF10 TL10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedInf.. |
|||
Flexural Modulus | 3.59 GPa | 521 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp DF002L PC LNP THERMOCOMP* DF002L is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Low Extractible.This data was supplied by SABIC-IP for the America.. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Teknor Apex Sinpolene GPP1620 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 20% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Chase Plastics CP Pryme® N120GL (COND, 50% RH) Nylon 6, 20% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Ecomass® 1005ZD96 Tungsten Powder Filled Co-Polyamide, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Co-Polyamide (COPA), Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing .. |
|||
Flexural Modulus | 3.59 GPa | 521 ksi | ISO 178 |
Ecomass® 1007ZC85 Stainless Steel Filled COPA Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsStainless Steel Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by Technical Poly.. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-20FG-0659 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-20FG-2153R 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FM-Y249B 30% Glass/Mineral Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.59 - 8.20 GPa | 521 - 1190 ksi | Average value: 5.46 GPa Grade Count:7 |
Overview of materials for Polyphenylene Ether, Glass/Graphite Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Glass/Graphite Reinforced". Each property range of values reported is minimum and m.. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | Tangent; ASTM D790 |
RheTech Products GC20P100-00UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.59 GPa | 520 ksi | Tangent; ASTM D790 |
RheTech Products GC20P105-08FA 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products. |