Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.15 GPa | 457 ksi | |
Quadrant EPP Nylatron® GSM PA 6 + MoS2, cast (ISO Data) Nylatron GSM contains finely divided particles of molybdenum disulphide to enhance its bearing and wear behaviour without impairing the impact and fatigue resistance inherent to unmodified cast nylo.. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Asia Pacific) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Dry Blend E7506 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon E7506 is recommended for whites and light pastel colors only. Performs well in extrusion blow molding and high rate fencing capstock applications.Physical properties based on Geon E7506 white 1.. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | |
Plastcom SLOVALEN PH 92 T 30 PP, 30% mineral filling FeaturesModified PP for injection moulding with the content of 30% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches.Packag.. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | 0.05 in/min; 3-point; ASTM D790 |
Americas Styrenics STYRON™ 666LR General Purpose Polystyrene Resin
(discontinued **) STYRON™ 666LR is a medium flow general purpose polystyrene specifically designed to blend with styrene butadiene styrene block copolymers for packaging applications requiring high clarity, improved.. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | ASTM D790 |
Qualchem Danaprop PP2GF-15 Polypropylene, 15% Glass Fiber Polypropylene (homo-polymer) reinforced with glass fiberInformation provided by Qualchem Zrt. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | ISO 178 |
Solvay TECHNYL® A 221 PA66, DRY Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | ISO 178 |
Solvay TECHNYL® A 225F PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.Available in: Europe, Latin America and North AmericaProduct.. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | ISO 178 |
Solvay TECHNYL® C 50 H2 PA6, DRY Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This p.. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EX00781H PEI LNP* THERMOCOMP* EX00781H is a compoud based on Polyetherimide containng Proprietary Filler(s). Added feature of this material is: Healthcare. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PKN4752 PPE+PS PPE+PS blend. High Heat. Translucent with yellow tint in natural color. FDA compliant. Extrusion and Injection Molding. Typical applications include High Performance Food Packaging, Electronics and .. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High heat. Extrusion. Microwavable. Food, electrical/electronic packaging uses. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | ASTM D790 |
CPC - Vycom FLAMETEC™ CPVC Chlorinated Polyvinyl Chloride Sheet Flametec™ CPVC made from Corzan® 4910 white 120 compound is a high heat, corrosion resistant chlorinated polyvinyl chloride sheet. Because of its excellent corrosion resistance at elevated tempera.. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | ISO 178 |
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, Conditioned Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
Flexural Modulus | 3.15 GPa | 457 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |