Mechanical Properties Metric English Comments
Flexural Modulus 22.7 GPa
3290 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66
LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Heat Stabilized...
Flexural Modulus 22.7 GPa
3290 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66 (Asia Pacific)
LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.
Flexural Modulus 22.7 GPa
3290 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA
LNP* LUBRICOMP* UCL36S is a compound based on Polyphthalamide resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Heat Stabilized, Electrically Con..
Flexural Modulus 22.7 GPa
3290 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP UCL36S PPA (Asia Pacific)
LNP* Lubricomp* UCL36S is a compound based on Polyphthalamide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Heat Stabilized, Electrically Cond..
Flexural Modulus 22.7 GPa
3290 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp LC008 PEEK (Europe-Africa-Middle East)
LNP* Thermocomp* LC008 is a compound based on Polyetheretherketone resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 22.7 GPa
3290 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66
LNP* LUBRICOMP* RCL36 is a compound based on Nylon 66 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wesr Resistant, Electrically Conductive.