Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200H High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200H is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200H High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200H is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200H High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200H is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200H High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200H is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABSPC 9901 ELG ABS/PC Injection Molding Grade, Very High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.618 - 3.044 GPa | 379.7 - 441.5 ksi | |
3D Systems Accura® 40 Plastic for SLA® Systems 40 Accura "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsHigh temperature testing:Automotive "under-the-hood" partsIntake manifoldsLighting components a.. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200H High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200H is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200H High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200H is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.618 GPa | 379.7 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |